Mark Cave breaks down how to safely handle inorganic lead runoff on glass and conservatory roofs without causing permanent damage. Learn why sodium hypochlorite fails, the risks to coated glass, and how to address the source using patination oil. Show Notes Lead X Pro Ready To Use Lead Stain Remove: https://www.softwashing.uk/products/lead-x-pro-ready-to-use-lead-stain-remover?srsltid=AYCX9vI32-mYs1hlJdQzRVdfdjj_MAmAeScFZqEWX7roZE7eEWyBT6JZ
Audio and video play straight from the show's own hosting. PodSubs stores and serves no media.
Transcript
From the show. Tap a time to play from there.
A customer rings you about a conservatory roof. Streaky white and grey marks running down the glass, right below a lead flashing. Your first instinct might be to reach for the softwash mix. Please don't. Because that stain is not green, it is not organic, and bleach is going to do absolutely nothing for it. I'm Mark Cave from SoftWash UK, and this one follows on from an earlier episode where we looked at metallic runoff under lead flashings on masonry. Today it moves onto glass.
And glass is a much less forgiving place to get it wrong. Let's start with what you're actually looking at. Fresh, unpatinated lead is exposed to rain. The rainwater leaches it, and what runs down is a chalky mineral deposit, basically lead carbonate and lead oxide. That is an inorganic, insoluble metallic deposit. It's not algae. It's not biofilm. Sodium hypochlorite works by oxidising organic matter, so there's simply nothing for it to attack here.
And it can make things worse. Sodium hypochlorite reacting with lead can turn the flashing brown or orange. So you've failed to clean the glass, and you've discoloured the lead above it. That's a fun phone call to make to the customer. Our own guidance is clear that hypo shouldn't be relied on for oil, rust, tannin, lead staining or heavy mineral deposits. Different problems, different chemistry. So what does remove metallic oxides? Traditionally, reducing or acidic chemistry, such as oxalic acid,
or specialist acidic formulations. There are also fine abrasive polishing compounds, cerium oxide based ones like Unger Rub Out. On masonry, that's a fairly familiar route with a test patch. On glass, it's a different story. Here's why. Plenty of modern rooflights, conservatory roofs and Velux style units carry factory coatings. Some are self-cleaning coatings, the photocatalytic, hydrophilic kind, titanium dioxide based, Pilkington Activ being the well known example.
Others are low-E thermal coatings. These layers are incredibly thin. Strong acid or an aggressive abrasive can etch, scratch, strip or cloud them. And once that happens, you can't clean it away. The glazing unit has to be replaced. Think about the numbers on that job. You were quoting for a cleaning price, and you've just created a glazing replacement. That's the consequence of treating glass like render. There's a second layer to it. Over many years, acidic mineral runoff can leach and bond into the glass itself.
So you may be dealing with mineral etching rather than a surface deposit. If that's the case, no chemical on earth will lift it, because it's no longer sitting on the glass. It's part of the surface. So how do you approach it professionally? First, identify. Is it a surface deposit or a permanent etch? Is the glass coated? If you can't confirm what the glass is, treat it as coated and be cautious. Check manufacturer guidance where you can. Second, if you do consider oxalic acid or a specialist lead remover,
start very weak. Small test patch, inconspicuous corner, strict control of dwell time. Watch it the whole time. The acid must never dry on the glass. And keep it off the rubber gaskets, aluminium frames and uPVC beads, rinsing immediately and thoroughly. Our Lead X Pro is designed for brown, orange and oxidised staining on lead surfaces, so it's really there for the flashing. Always read the label and the safety data sheet, and test before you go near
anything else. Third, and this is the one people skip, deal with the source. If raw lead is still sitting above that glass, it will bleed fresh deposits on the very next shower. You can clean it beautifully on Friday and the customer's ringing you on Tuesday. Treating the lead, for example with a patination oil, helps seal the metal and slows the runoff. Otherwise you're just cleaning on repeat. Fourth, be honest with the customer. Results on glass can't be guaranteed. Document the existing condition with photos, explain the limitations before you
start, and get a signed acknowledgement. Never promise like new glass. I'd rather lose a job than win one on a promise I can't keep. This is really what professional softwashing is about. Knowledge comes before products. A strong chemical and a good pump are useless if you haven't diagnosed the stain and understood the surface. Podcasts like this are a great start, but if you're serious, the CPD Certified Softwash Training Course at softwashing.uk goes much deeper into
chemical selection, surface identification, safety and pricing work correctly. You learn online at your own pace, and you can become an Approved Softwash Applicator, with a directory listing and a place in the National Association of Softwash community. So here's your challenge. Next time you see white streaks under lead, stop before you reach for anything. Ask three questions: what is it, what is the glass, and where is it coming from? Answer those, and you'll avoid the costly mistakes.
We break down the 20 November 2026 UK-EU agreement to align Great Britain with EU biocidal regulations from March 2028, explaining why current rules for sodium hypochlorite and DDAC remain unchanged today. Plus, we...
Mark Cave from SoftWash UK explains how to assess roof hazards, follow the three-step access hierarchy, and select the safest cleaning method between biocide treatments and sodium hypochlorite. Show Notes Health and...
Mark Cave explains why newly installed concrete driveways, Indian sandstone patios, and rendered facades are often at their most vulnerable. Learn the difference between drying and curing, how to handle efflorescence...
Mark Cave explains why certainty in exterior cleaning Facebook groups is often mistaken for competence and highlights the red flags of bad chemical advice. Learn how to spot trustworthy, evidence-based guidance by...
Mark Cave explains why sodium hypochlorite is not a universal cleaner and how to calculate dilutions from actual stock strength for organic contamination. Learn essential site controls, PPE requirements, chemical...